Phone, Telegram, WhatsApp, Viber

Mixture mantry clan-sand heat-resistant "stove" 5.0 kg

Product Code: 7994554
$9.00
In Stock
Characteristics
A country
Russia
Application
For interior and exterior use
Appointment
For heating devices
View
Mixture
Weight, kg
5
...

The composition

is chamotene clay, quartz sand.

properties

heat -resistant, environmentally friendly, high -plastic pantry. The heat resistance of the mixture is +1350 ° C.

The purpose

is used for masonry and repair of external and internal elements of household furnaces, fireplaces, chimneys from ceramic and fireproof brick.

Preparation of the base

for masonry, it is recommended to use red ceramic brick. The brick should be cleared of dust, dirt, soot, adhesive masses and plaster. Red ceramic brick before masonry is recommended to moisten abundantly with water. Moorpicat is not required for a variable brick.

preparation of a solution

to obtain a finished solution, it is necessary to mix a dry mixture with clean water in a ratio of 0.25-0.28 l per 1 kg of a mixture (5 , 0 - 5.6 liters per bag 20 kg) until a homogeneous mass is obtained without lumps. The resulting mortar mixture is withstand for 15-20 minutes, then mix again.

the performance of the work

of the work is carried out at a temperature of +5 ° C to +60 ° C. Recommended thickness of the pantry of 3-10 mm. It is necessary to apply the solution with a trowel or a cell, the seams of the seams by bricks are carried out immediately during the panting work.

when thickened the solution, it is necessary to add water and mix. When performing external works, it is recommended to add cement to the finished solution.

Drying of the finished furnace

After the stove is erected in the seams of the masonry and brick, a significant amount of moisture remains. Therefore, after the complete end of the panting work, the ignition and operation of the finished furnace is strictly prohibited. The first heating is recommended no earlier than 48 hours from the end of the masonry work to a temperature of not higher than +300 ° C. For 3-7 subsequent days, depending on the size of your furnace, it is necessary to burn a small amount of fuel (wood chips, dry branches) in the furnace furnace at least twice a day for 1-1.5 hours. As the furnace dries, the amount of fuel must be increased. At the same time, all doors (furnace, blowing, food) and valves should be open. This is necessary for removing water vapor from masonry.

Technical characteristics

The color of the mixture: Gray

The time of use of the solution: not limited

temperature Applications: from +5 ° C to +60 ° C

Complete drying time: at least 72 hours

Recommended layer thickness: 3-10 mm

heat resistance : +1350 ° C

water consumption for preparing l/kg: at least 0.25 l.

Characteristics
A country Russia
Application For interior and exterior use
Appointment For heating devices
View Mixture
Weight, kg 5
Write a review
Note: HTML is not translated!

There are no reviews for this product.

Tags: Heat -resistant mixtures (bath and sauna), heat -resistant mixtures (construction and repair), heat -resistant mixtures (construction and repair)