Repair heat -resistant mixture for stoves and fireplaces "stove" 3.0 kg
The purpose
The dry mixture is designed to prepare a construction solution used to repair household furnaces and fireplaces.
Attention! Suitable for repairing furnaces made of ceramic and refractory brick.
composition
fire -controlled fillers, fractionated sand, cement knitting, mineral fillers, modifying polymer additives.
Preparation of the base
Attention! The properties of the product are guaranteed only with strict adherence to recommendations for preparation for work.
before the start of repair work, the surface of the furnace is cleaned of dust, soot, residues of the panting solution or clay. If necessary, the repair sites are wiped with a damp rag.
the preparation of the solution
to obtain the finished solution, it is necessary to dilute 1 kg of dry mixture into 0.21-0.22 liters of clean tap water. Mixing is better in a mechanized way (a drill with a nozzle) or manually, evenly pouring a dry mixture into the water until a homogeneous pasty mass is obtained. Take the solution for 10-15 minutes, stirring slightly. After that, mix secondly and the material is ready for use. To prepare the solution, use only clean water that does not contain suspended particles and dissolved salts.
Attention! The finished solution must be used within 30 minutes, a longer period leads to a decrease in the strength of the finished product. Use a thickening solution, re -diluting it with water, is not allowed.
The order of work
Attention! For fire safety purposes, it is forbidden to carry out repair work during the stoves. Large potholes on brick, seams and cracks are filled with a finished solution to the entire depth. At the end of the repair work, the excess of the solution must be removed. With the complete destruction of individual brick in the laying of the furnace, it should be replaced using this repair mixture. When replacing a large amount of brick, use the masonry mixture for stoves and fireplaces "stove". One day after the end of repair work, the surface of the furnace can be plastered with plaster for stoves and fireplaces "stove" or lined with tiles (stone, tiles), using glue heat -resistant for stoves and fireplaces "
attention! Increased humidity and low temperatures can increase the drying time of repaired fragments of the furnace.
Consumption
The consumption of the finished solution directly depends on the volume of repair work performed.
| Characteristics | |
| A country | Russia |
| View | Stoves-stone |
| Weight, kg | 3 |